| Base Fabric Type |
Polyester
|
|
| Base Fabric Weight (nominal) |
3.0 oz/yd2
|
100 g/m2 |
| Finished Coated Weight ASTM D751 |
30.0 +2/-1 oz/yd2 | 1020 ±35 g/m2 |
| Tongue Tear ASTM D751@12 in/min |
60/60 lb 8" x 10" sample |
266/266 N 20 cm x 25 cm sample |
| Grab Tensile ASTM D751 |
230/200 lb | 1020/890 N |
| Strip Tensile ASTM D751, Procedure B |
200/140 lb/in | 890/620 N/cm |
| Adhesion (minimum) ASTM D751, Dielectric Weld |
7.0 lb/in | 30 N/2.5 cm |
| Hydrostatic Resistance ASTM D751, Procedure A |
500 psi | 340 N/cm2 |
| Low Temperature ASTM D-2136 LTC 1/8" Mandrel 4 hrs |
Pass -40° F | Pass -40° C |
| Flame Resistance Method 4910 MFR |
Sample not consumed within 2 minutes | |
| Dead Load Room Temperature 160° F. |
2" overlap seam 100 lb 50 lb |
445 N @ 21° C 220 N @ 70° C |
We believe this information is the best currently available on the subject. We offer it as a suggestion in any appropriate experimentation you may care to undertake. It is subject to revision as additional knowledge and experience are gained. We make no guarantee of results and assume no obligation or liability whatsoever in connection with this information. In case of conflict between standard and metric specifications, standard shall apply.